Precious Metal Clay


pmc

Click to enlargePMC3 - 9 gram, Syringe
Extrudes a string like shape. Includes a tip that can be trimmed to allow different extrusion gauge.

pmc-syringe
Click to enlargePMC3 - Moist, 50 grams
Shape this as you would regular clay. Shrinage is 8 - 10 %. Firing temp is 1110F - 1290F. Weight is net silver.

pmcmoist-50
Click to enlargePMC3 Paste - 15 grams
Very versatile,can be used to coat organic objects such as a leaf tocreate an exact image after PMC is fired.

pmcslip-15
Click to enlargePMC3 Moist - 16grams
pmcmoist16
Click to enlargePMC+ Moist - 45 gram
pmcmoist45
Click to enlargePMC+ Moist - 18 gram
pmcmoist-18
Click to enlargePMC+ Paste - 18 gram
pmcslip-18
Click to enlargePMC+ Sheet - 5 gram
A flat 2 3/8" square. Cut with sissors or razor knife, or tear it to acchieve a ragged edge. Join elements by using PMC paste like a glue. Additonal instruction included.

pmcsheet5
Click to enlargeCork Clay, 8 oz.
Is used to form and hold the shape while being fired. Let cork clay dry before firing. Use only on items fired in a well ventalated kiln because of toxic fumes given off by cork clay. Do not exceed 1472F as cork clay burns hot and may cause silver to melt if fired at higher temperatures. Store in airtight container, a zip lock bag works well.

corkclay8
Kilns for precious metal - look at the Olympic kilns page.
newitem73856638
Cork Clay - 4 oz.
corkclay4oz